Brandenburg, Germany

Lindhof Agri-PV

Vertical bifacial rows over grazing land. Nine cell-level hot spots, most on rows the sheep rub against.

Black-hot thermal frame of Lindhof Agri-PV with the hot spot marked

TRK 0352

58.2 °C

9 contacts

52.3906° N 13.0645° E

ALT 48 m AGL · HDG 006° · 10:41 UTC

Black-hot thermal frame of Lindhof Agri-PV with the hot spot marked

TRK 0352

58.2 °C

9 contacts

52.3906° N 13.0645° E

31

ha

Area covered

29

min

Flight time

9

flagged

Anomalies found

58

°C

Hottest reading

Findings

  • Rows 3 and 4: six cracked cells at 52–58 °C, likely mechanical damage

  • One junction box at 58.2 °C on row 11

  • No PID pattern detected across the array

Debrief

Vertical modules need an oblique pass, so the flight plan switched to 35° camera pitch and flew both faces of every row.

Findings were grouped by row so the farm crew could replace damaged modules during the next shearing break.

The east and west faces come back as separate contacts, which is the only way we can tell where the damage actually is.

Jonas Weber, site manager

Next contact

Coldharbour Solar

Coldharbour Solar

End of feed · CH2

© 2026 Isotherm Systems

End of feed · CH2

© 2026 Isotherm Systems

Create a free website with Framer, the website builder loved by startups, designers and agencies.